Still deciding? Get samples of $ !
Order Sample
|
| Customization: | Available |
|---|---|
| Application: | Woodworking |
| Bonding Function: | Instant Adhesive |
| Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
|---|
| Payment Methods: |
|
|---|---|
| Support payments in USD |
| Secure payments: | Every payment you make on Made-in-China.com is protected by the platform. |
|---|
| Refund policy: | Claim a refund if your order doesn't ship, is missing, or arrives with product issues. |
|---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
| Shanghai Angmi New Material Technology Co.,ltd | ||||
| Technical Data Sheet | ||||
| Item No.: 6166 (High Temperature Hot Melt glue) | ||||
Items: |
Cream/beige color,Non-toxic and environmental friendly.Main components are ethylene andvinyl acetate, added with tackifying resin, accelerator'promoter, stuffing etc. |
|||
Technical Data: |
viscosity number: 200ºC | Density: 1.20g/cm3 | ||
| softening point: 100-105ºC | heat-resistant Point>60ºC | |||
Operation Data: |
Material humidity≥15ºC Ambient temperature ≥15ºC |
Moisture Content: 8%- 10% | Pot/Tank Temperate :170- 180ºC | |
| Rubber Roller Temperate:180- 210ºC | Pressure:3-5kg/cm3 |
Speed>15meters/min |
||
Application : |
Applicable for large full-automatic Linear edge banding machine ;Suitable for PVC,ABS and other edge banding materials; |
|||
Characters: |
1.Suitable for majority of large automatic edge banding machines ; |
2.High thermal resistance,high strength, resistance to low temperature ; | ||
| 3.Good liquidity,looks good and very little waste; | ||||
| HOW TO USE AND NOTES:: | ||||
| 1. Have knowledge of different kinds of hot-melt glue and their technical Characters( including technical data). | ||||
| 2.Temperate of Hot melt adhesive pot should be controled in the range of using temperate. | ||||
| 3.Should have periodic cleaning for Preheating glue pot to keep cleaness of the pot. | ||||
| 4.Boards and edging materials should be avoid of being polluted. | ||||
| 5.Moisture content of the boards should be around 8%- 10%. | ||||
| 6.Putting proper quantity of glue into the glue pot/pan , if putting too much, could make the glue deteriorate , and with less viscosity . |
||||